Hey everyone, I am trying to get my piece of junk Tiertime UP Mini 2 printer to work somewhat reliably, but it also is my first printer, so I don’t have a lot of practice with debugging these things. While flushing some PLA through the Hot End (without a nozzle) I noticed that it looks very bubbly at temperatures between 195°C and 210°C (see picture above) and I wondered if this should tell me that I have been printing too hot. With lower temperature (160°C) the film looks pretty smooth (see second picture below) but that sounds way too low to actually print PLA with. I now tried printing with my 0.4mm nozzle at 190°C, but had no adhesion on the bed. It was no better at 200°C. Both times the bed was at about 55°C. Is there something I do fundamentally wrong or is that a normal texture for PLA after heating? I would have printed a temperature tower, but firstly I have no adhesion on the first layer and secondly I do not think I can set different temperatures for different regions in the Tiertime slicer I have to use with this printer. Usually I would like to try out a bunch of things, but before I sink hours into this and clog my nozzle really badly again, I wondered if any of you has some suggestions.

Context: I am working on this on and off for the last year, but it is quite frustrating, because with each clogging I need so much time to get the nozzle and hot end free again. I got the printer for free and its form factor fits perfectly into one space I have free in my apartment. The printer came loaded with ABS, but I didn’t like the smell in combination with air filter, that has never been changed. So I figured PLA would be better for a beginner. Maybe my problems started there, because I didn’t consider that cleaning might be necessary for the switch. I was able to get a fine benchy out of there a couple of times but usually after 3 or four prints, I get clogging in the heating element (I suspect heat creep being an issue). So right now I have some flow through the hot end again after I cleaned it over a couple of days with cycles of soaking in acetone and picking out softened PLA. When doing a couple of cold pulls with a cleaning filment by eSun at 110°C, I noticed the behaviour described above. I also exchanged the nozzle once although that one might be messed up now as well. A couple of times the prints failed by not extruding anything anymore and liquid PLA coming out between hot end and nozzle. But last time, I am pretty sure the clog was higher, somewhere inside the hot end, which is why I did this long solvent cleaning.

I am happy about any help and tips you might have!

  • marcos@lemmy.world
    link
    fedilink
    English
    arrow-up
    24
    ·
    6 days ago

    The bubbles are probably because your filament is moist, and are not related to the clogging.

    If you have been printing with PLA for a while, the ABS it had originally shouldn’t be a problem. Look if the hot-end is clean, and if its heat dissipater has enough airflow. It’s quite hard to discover the cause of clogs, but I’d start there.

    • Kratzkopf@discuss.tchncs.deOP
      link
      fedilink
      English
      arrow-up
      2
      ·
      5 days ago

      Thanks, the part about ABS is a relief, I was worried I contaminated that thing for good. I will also take a look at the air flow and try to get a filament dryer.

  • artyom@piefed.social
    link
    fedilink
    English
    arrow-up
    6
    ·
    6 days ago

    Bubbles are an indicator of moist filament. Get a drier. Sometimes you can use an oven if the temps go low enough.

  • autriyo@feddit.org
    link
    fedilink
    English
    arrow-up
    4
    ·
    6 days ago

    I don’t know how your hot end is constructed, but on the cheap e3d clones its easy to accidentally undo the gap(heatbreak) between the heating block and the heatsink while changing nozzles.

    Especially when dealing with clogged/stuck stuff. I’ve been chasing clogging issues on mine for a while, which eventually turned into failure to heat problems.

    And only after ruling out nearly everything else did I notice that the gap/heatbreak was not there anymore. Which is constrained only by screwing things together the right amount, when fighting with clogs constantly, its kinda easy to lessen that gap slightly every time.

    • Kratzkopf@discuss.tchncs.deOP
      link
      fedilink
      English
      arrow-up
      2
      ·
      3 days ago

      Thanks very much, that is also good input! I think there is quite some room for the heat sink to be badly aligned, as the heating element can wriggle a bit down and up and is not super firmly fixed. This was a parameter I had not yet considered. Is there in your experience more clogging if the heat sink overlap is too small or too big? I consider adding a bit of heat conducting pate to improve cooling.

      I misunderstood you at first and thought of the gap between nozzle and heater, which might also be a problem with the internal screw in my setup. So I gave it in another clean and have hope that the nozzle is better heated through now.

      • autriyo@feddit.org
        link
        fedilink
        English
        arrow-up
        1
        ·
        3 days ago

        Gap looks big enough. I don’t think you can really have too big, at least without modifying.

  • thisbenzingring@lemmy.today
    link
    fedilink
    English
    arrow-up
    3
    ·
    6 days ago

    by a cheap food dehydrator and dry out your filament before using, that will probably solve the bubbles and stringing after the print

    but you might also consider a fresh nozzle head, unless you get a tungsten steel head, it will need to be replaced every so often. the brass nozzles wear out and start producing junk prints